Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 220.6 GPa | 31990 ksi | |
Latrobe Lescalloy® BG42 VIM-VAR High Performance Bearing Steel LESCALLOY BG42 VIM-VAR steel is a martensitic, stainless high speed steel that combines the tempering, hot hardness and hardness retention characteristics of M50 high speed steel with the corrosion .. |