Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 216 GPa | 31300 ksi | |
Poco Graphite SUPERSiC® 3C Silicon Carbide SUPERSiC that has been coated with a 75 µm CVD SiC coating, which seals the surface.Uses: Ideal for high-temperature deposition and CVD applications.Information provided by PocoGraphite |
|||
Modulus of Elasticity | 216 GPa | 31300 ksi | |
Poco Graphite SUPERSiC® 3CX Silicon Carbide SUPERSiC that has been coated twice with a 75 µm CVD SiC coating, which seals the surface. Uses: Ideal for high-temperature anneal processesInformation provided by PocoGraphite |
|||
Modulus of Elasticity | 216 GPa | 31300 ksi | |
Poco Graphite SUPERSiC® Basic Silicon Carbide The SUPERSiC Material System allows customization of basic silicon carbide. Select from groups of infiltration materials, cleaning options, coating materials and thicknesses to optimize material for.. |
|||
Modulus of Elasticity | 216 GPa | 31300 ksi | RT |
Haynes Hastelloy® B-3® alloy, 0% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Modulus of Elasticity | 216 GPa | 31300 ksi | RT |
Haynes Hastelloy® B-3® alloy, 10% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Modulus of Elasticity | 216 GPa | 31300 ksi | RT |
Haynes Hastelloy® B-3® alloy, 20% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Modulus of Elasticity | 216 GPa | 31300 ksi | RT |
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Modulus of Elasticity | 216 GPa | 31300 ksi | RT |
Haynes Hastelloy® B-3® alloy, 30% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Modulus of Elasticity | 216 GPa | 31300 ksi | RT |
Haynes Hastelloy® B-3® alloy, 40% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Modulus of Elasticity | 216 GPa | 31300 ksi | RT |
Haynes Hastelloy® B-3® alloy, 50% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Modulus of Elasticity | 216 GPa | 31300 ksi | RT |
Haynes Hastelloy® B-3® alloy, 6.3 mm plate The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Modulus of Elasticity | 216 GPa | 31300 ksi | RT |
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea.. |