Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.219 GPa | 31.8 ksi | Molded Sample 2% Secant Modulus |
Dow DOWLEX™ 2505 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2505 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with good rigidity. It has ex.. |