Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 7.60 - 21.0 GPa | 1100 - 3050 ksi | Average value: 11.1 GPa Grade Count:7 |
Overview of materials for Phenolic, Novolac, Impact Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum .. |
|||
Modulus of Elasticity | 0.470 - 21.0 GPa | 68.2 - 3050 ksi | Average value: 5.79 GPa Grade Count:83 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |