Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 209.9 GPa | 30450 ksi | (hardened to 62 HRC) |
Bohler-Uddeholm AISI D2 Cold Work Tool Steel AISI D2 is a high-carbon, high-chromium tool steel alloyed with molybdenum and vanadiumAISI AD2 is characterized by: High wear resistance High compressive strength Good through-hardening properties.. |