Polymer Property : Modulus of Elasticity = 30160 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 207.9 GPa
30160 ksi
496°C Temper Temperature
Latrobe CSS-42Lâ„¢ VIM-VAR High Performance Carburizing Stainless Steel; Bearing and Gear Steel
CSS-42L™ is a case carburizable stainless steel alloy intended to be used at operating temperatures up to 800°F (427°C). The alloy is able to achieve and maintain a high surface hardness ..