Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.94 GPa | 572 ksi | Cross; ASTM D638 |
Arlon CuClad 250 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate CuClad 250 uses a higher fiberglass/PTFE ratio to provide mechanical properties approaching those of conventional substrates. Better dimensional stability and lower thermal expansion in all directi.. |