Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.360 - 3.75 GPa @Temperature -40.0 - 120 °C |
52.2 - 544 ksi @Temperature -40.0 - 248 °F |
Average value: 1.69 GPa Grade Count:4 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |