Modulus of Elasticity 3.17 GPa
460 ksi
ASTM D638
NOVA Chemicals Dylark® 232 High Performance Styrenic, Transparent Grade
High heat resistance, Sparking water-white clarity, Good chemical resistance, High modulus, for superior shear and torque resistanceApplications: Light pipes and lighting, High heat microwave packag..
Modulus of Elasticity 3.17 GPa
460 ksi
ASTM D638
Technetics Group Amicon™ PET-P  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)