Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.068 GPa | 445.0 ksi | ASTM D638 |
Ineos Nova 2581 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Good balance of flow, strength and heat resistanceApplications: Consumer electronics, HousewaresExposure to gamma radiation in the 2.02-6.06 megarad range has no significant eff.. |