Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 205 GPa | 29800 ksi | |
Crucible Steel 422 Stainless Steel Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is.. |
|||
Modulus of Elasticity | 205 GPa | 29800 ksi | (hardened to 60 HRC) |
Bohler-Uddeholm UDDEHOLM VANADIS 4 EXTRA® Powder Metallurgically Produced Tool Steel Description: Uddeholm Vanadis 4 Extra is a chromiummolybdenum-vanadium alloyed steel Vanadis 4 Extra is characterized by: Very good ductility High abrasive-adhesive wear resistance High compressive.. |