Polymer Property : Modulus of Elasticity = 2830 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 19.5 GPa
2830 ksi
DIN 53 457
Albis Plastics Tedur® L 9521-1 PPS, 60% Glass Fiber/Mineral  (discontinued **)
Extremely Rigid. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Sockets, Plugs and HandlesProcessing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperatur..