Polymer Property : Modulus of Elasticity = 2800 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 19.3 GPa
2800 ksi
Y; ASTM D3039
Park Electrochemical Nelco® N4000-7 FR-4 Epoxy Laminate and Prepreg
The Nelco® N4000-7 low-CTE epoxy laminate and prepreg system is a cost-effective solution for use in a broad range of multilayer PCB designs requiring low Z-axis expansion, excellent thermal stabil..
Modulus of Elasticity 19.3 GPa
2800 ksi
SGL Carbon Group EK 2240 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Modulus of Elasticity 19.3 GPa
2800 ksi
SGL Carbon Group EK 2241 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Modulus of Elasticity 19.3 GPa
2800 ksi
IPC TM-650 2.4.18.3
Arlon 45N Multifunctional Epoxy Laminate and Prepreg
Arlon 45N is a tough, high Tg (175°C by DSC) multifunctional epoxy laminate and prepreg system designed for use in a variety of higher layer count MLBs. Processable using conventional FR-4 conditi..
Modulus of Elasticity 19.3 GPa
2800 ksi
IPC TM-650 2.4.18.3
Arlon 44N Multifunctional Microdispersed Ceramic Filled Epoxy-Fiberglass Prepreg
Arlon 44N is a high resin content multifunctional (175°C) epoxy prepreg system with a proprietary microdispersed ceramic filler system. 44N is engineered for the filling of clearance holes in thi..