Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 18.615 GPa | 2699.9 ksi | |
Sawbones Second-Generation Simulated Cortical Bone E-glass / Epoxy CompositeSawbones® Second-Generation composite bone is a combination of e-glass cloth, mat, and roving, layered around a rigid polyurethane foam core, which models the cancellous .. |