Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 180.6 GPa @Temperature 482 °C |
26190 ksi @Temperature 900 °F |
|
Latrobe Lescalloy® BG42 VIM-VAR High Performance Bearing Steel LESCALLOY BG42 VIM-VAR steel is a martensitic, stainless high speed steel that combines the tempering, hot hardness and hardness retention characteristics of M50 high speed steel with the corrosion .. |