Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.69 GPa | 245 ksi | ISO 527 |
GEHR Plastics ECTFE Polyethylene Chlorotrifluoroethylene Ethylene-Chlortrifluorethylene exhibits an extraordinary impact strength at temperatures ranging from -76°C to 150°C. A great part of the product properties attributes to the very smooth surfa.. |
|||
Modulus of Elasticity | 1.69 GPa | 245 ksi | ASTM D882-83A (mod) |
Lord Adhesives Fusor® 310 A/B Epoxy Adhesive Lord® 310 adhesive is a modified, thixotropic, two-part epoxy adhesive which bonds well to many types of prepared metals, prepared rubber, urethane, and plastics. Originally formulated for primer.. |