Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 231 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 231 GPa
33500 ksi
Tensile modulus calculated at secant 6000-1000
Hexcel® AS4C Carbon Fiber (12,000 Filaments)
Weight/length = 0.800 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..
Modulus of Elasticity 231 GPa
33500 ksi
Tensile modulus calculated at secant 6000-1000
Hexcel® AS4C Carbon Fiber (3000 Filaments)
Weight/length = 0.200 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..
Modulus of Elasticity 231 GPa
33500 ksi
Tensile modulus calculated at secant 6000-1000
Hexcel® AS4C Carbon Fiber (6000 Filaments)
Weight/length = 0.400 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..
Modulus of Elasticity 231 GPa
33500 ksi
In Tension
Cytec Thornel® T-300 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..
Modulus of Elasticity 231 GPa
33500 ksi
In Tension
Cytec Thornel® T-300 1K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..
Modulus of Elasticity 231 GPa
33500 ksi
In Tension
Cytec Thornel® T-300 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..
Modulus of Elasticity 231 GPa
33500 ksi
In Tension
Cytec Thornel® T-300 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..
Modulus of Elasticity 231 GPa
33500 ksi
Bohler-Uddeholm BÖHLER S390 MICROCLEAN® High Speed Steel
Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug..
Copyright © lookpolymers.com All Rights Reserved