Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.463 - 7.35 GPa @Temperature -40.0 - 150 °C |
212.2 - 1070 ksi @Temperature -40.0 - 302 °F |
Average value: 4.15 GPa Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |