Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 202.5 GPa | 29370 ksi | |
Assab Steels 8407 2M Hot Work Steel ASSAB 8407 is a chromium-molybdenum-vanadium-alloyed steel which is characterized by: Good resistance to abrasion at both low and high temperatures. High level of toughness and ductility Uniform .. |
|||
Modulus of Elasticity | 202.5 GPa | 29370 ksi | |
Assab Steels QRO 90 SUPREME Hot Work Steel QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista.. |
|||
Modulus of Elasticity | 202.5 GPa | 29370 ksi | |
Assab Steels 8407 SUPREME Hot Work Steel 8407 SUPREME is characterized by:High level of resistance to thermal shock and thermal fatigueGood high temperature strengthExcellent toughness and ductility in all directionsGood machinability and .. |