Mechanical Properties Metric English Comments
Modulus of Elasticity 0.138 GPa
20.0 ksi
Secant; ASTM D638
Huntsman PE1753 EVA Film Extrusion  (discontinued **)
7.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with good clarity and excellent impact strength.Applications: Film extrusion: icebags, liquid packaging, lamination film, and ..