Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.896 GPa | 420.0 ksi | ASTM D638 |
Ineos Nova 1531 High Heat Crystal Polystyrene
(discontinued **) High flow and high heat resistance, Excellent clarityApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optical p.. |
|||
Modulus of Elasticity | 2.896 GPa | 420.0 ksi | ASTM D638 |
Ineos Nova 1504 High Heat Crystal Polystyrene Good balance of flow, strength and set up properties, Blue edge effect, USP Class VIApplications: Consumer electronics, Housewares, Cosmetic packagingExposure to gamma radiation in the 2.02-6.06 meg.. |
|||
Modulus of Elasticity | 2.896 GPa | 420.0 ksi | |
KYDEX® 6565 Acrylic/PVC Thermoplastic Sheet Low heat release aviation gradeApplications: Airducts, seat parts, bulkhead laminates, escape slide packboards, gallery parts, instrument panels, laboratory floorplans, sidewall panels, life vest sh.. |