Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.70 - 2.86 GPa | 247 - 415 ksi | Average value: 2.49 GPa Grade Count:19 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |