Mechanical Properties Metric English Comments
Modulus of Elasticity 1.10 - 2.69 GPa
160 - 390 ksi
Average value: 1.93 GPa Grade Count:16
Overview of materials for PETG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Modulus of Elasticity 1.00 - 2.69 GPa
145 - 390 ksi
Average value: 1.80 GPa Grade Count:22
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..