Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0180 - 0.207 GPa
2.61 - 30.0 ksi
Average value: 0.0508 GPa Grade Count:9
Overview of materials for Styrenic Elastomer (TES)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro..
Modulus of Elasticity 0.0180 - 0.0680 GPa
2.61 - 9.86 ksi
Average value: 0.0313 GPa Grade Count:8
Overview of materials for Styrenic TPE  (Unverified Data**)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe..
Modulus of Elasticity 0.0180 - 0.0800 GPa
2.61 - 11.6 ksi
Average value: 0.0474 GPa Grade Count:9
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Molding Grade". Each property range of values reported is minimum an..
Modulus of Elasticity 0.0180 GPa
2.61 ksi
ASTM D412
KKPC KOSYN KTR 302 Thermoplastic Elastomer (TPE)
Thermoplastic Elastomer (TPE)Characteristics: KOSYN KTR101 is linear block copolymer made by solution polymerization which polymerizes butadiene and styrene in organic solvent. It is thermoplastics ..