Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0160 GPa | 2.32 ksi | |
Mitsui NOTIO™ PN-2070 Nano-crystal Structure Controlled Elastomer NOTIO™ is a polyolefin elastomer designed by a really new concept. NOTIO™ is a controlled crystal and amorphous structure on a nano scale, and shows better properties when compared with conventio.. |