Polymer Property : Modulus of Elasticity = 2.207 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.207 GPa
320.1 ksi
ASTM D638
Ineos Nova 5100 High Impact Polystyrene  (discontinued **)
Good balance of toughness and rigidity, USP Class VIApplications: Spools and reels, Thermoformed and molded packaging, Photographic cartridges, AppliancesProperties were determined on injection mold..
Modulus of Elasticity 2.207 GPa
320.1 ksi
ASTM D638
Ineos Nova 5104 High Impact Polystyrene  (discontinued **)
Good balance of toughness and rigidity, USP Class VIApplications: Spools and reels, Thermoformed and molded packaging, Photographic cartridges, AppliancesProperties were determined on injection mold..