Polymer Property : Modulus of Elasticity = 18.7 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 18.7 GPa
2710 ksi
ASMT D638
Toyobo TS501 PPS, 50% Glass Fiber Reinforced
Key Feature: High stiffnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent physical, e..
Modulus of Elasticity 18.7 GPa
2710 ksi
ISO 527-2
BASF Ultradur B 4040 G10 BK5110 50% Glass Filled PBT
Injection-molding grades containing 50% of glass fibers, for industrial parts with excellent surface quality.Applications: External door handles in vehicles, visible sunroof frames, over door handle..