Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.654 - 10.89 GPa @Temperature -20.0 - 250 °C |
94.9 - 1579 ksi @Temperature -4.00 - 482 °F |
Average value: 4.47 GPa Grade Count:2 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |