Mechanical Properties Metric English Comments
Modulus of Elasticity 4.00 - 10.8 GPa
580 - 1560 ksi
Average value: 7.53 GPa Grade Count:27
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..