Polymer Property : Modulus of Elasticity = 15.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.104 GPa
15.1 ksi
ASTM D638
Arkema Group LOTADER® AX 8840 Copolymer Ethylene - Glycidyl Methacrylate
LOTADER AX 8840 is a random copolymer of Ethylene and Glycidyl Methacrylate, polymerized under high pressure in an autoclave process. Due to the reactivity induced by the Glycidyl methacrylate, LOTA..