Polymer Property : Modulus of Elasticity = 1390 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 4.50 - 9.60 GPa
653 - 1390 ksi
Average value: 7.77 GPa Grade Count:3
Overview of materials for Phenolic/Rubber; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp..