Mechanical Properties Metric English Comments
Modulus of Elasticity 50.0 - 90.0 GPa
7250 - 13100 ksi
at constant voltage
ETREMA Products Terfenol-D Magnetostrictive Smart Material (Tb0.3Dy0.7Fe1.92)
Terfenol-D is the commercial name for Tb0.3Dy0.7Fe1.92; a composition of material that exhibits giant magnetostriction.Magnetostriction is the phenomenon in which an applied magnetic field causes an..