Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 8.80 - 8.80 GPa @Temperature 80.0 - 80.0 °C |
1280 - 1280 ksi @Temperature 176 - 176 °F |
Average value: 8.80 GPa Grade Count:1 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |