Mechanical Properties Metric English Comments
Modulus of Elasticity 3.03 - 8.69 GPa
440 - 1260 ksi
Average value: 4.49 GPa Grade Count:13
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl..