Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.600 - 8.31 GPa @Temperature -40.0 - 150 °C |
87.0 - 1210 ksi @Temperature -40.0 - 302 °F |
Average value: 3.50 GPa Grade Count:5 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |