Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 75.0 GPa | 10900 ksi | |
PEAK Werkstoff DISPAL S691 Aluminum Alloy, AlCu5Ti High stiffness and elongation at ruptureInformation provided by PEAK Werkstoff GmbH |
|||
Modulus of Elasticity | 75.0 GPa | 10900 ksi | Young's Modulus |
Momentive Performance Materials Type 219 Fused Quartz Tubing Known as "Ozone-Free" or "Germicidal" quartz tubing. Transmits UV-A and UV-B while blocking the deep, high energy wavelengths that cause ozone generation and pose the greatest exposure risks. Tran.. |
|||
Modulus of Elasticity | 75.0 GPa | 10900 ksi | |
Schott Glass 8326 Neutral Glass Tubing Neutral glass tubing, alkali resistance better as for DURAN® Special lab glass The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is less than 100 ppm.Info.. |