Polymer Property : Modulus of Elasticity = 1089 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 7.508 GPa
1089 ksi
MD; ExxonMobil Method
ExxonMobil Metallyte™ 38MW280 OPP Film
Product Description: A super white opaque biaxially oriented polypropylene film, metalized on one side. Ideal for single web packaging applications on HFFS in combination with cold seal.Availability..