Polymer Property : Modulus of Elasticity = 1060 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 7.30 GPa
1060 ksi
ASTM D638
Toyobo T-422-02R Nylon, Mineral-Reinforced
Key Feature: High heat distortion and good toughness, high flowInformation provided by Toyobo Co., Ltd
Modulus of Elasticity 7.30 GPa
1060 ksi
ISO 527-2
BASF Ultraform® N2200 G43 POM
Description: Is a POM, injection-molding grade for parts requiring high stiffness and strength together with good mold release.Information provided by BASF