Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.05 - 1.85 GPa | 152 - 268 ksi | Average value: 1.59 GPa Grade Count:9 |
Overview of materials for Cellulose Acetate Propionate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val.. |