Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.35 - 1.79 GPa | 196 - 260 ksi | Average value: 1.59 GPa Grade Count:15 |
Overview of materials for Polypropylene, Fiber Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app.. |