Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.25 GPa | 181 ksi | ISO R527 |
Arkema Group Orgalloy® LE 60 ES Polyamide Alloy Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group |
|||
Modulus of Elasticity | 1.25 GPa | 181 ksi | ISO 178 |
Addiplast Addilene H 210 Polypropylene Homopolymer UnreinforcedInformation provided by Addiplast. |