Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.17 - 16.0 GPa | 170 - 2320 ksi | Average value: 4.07 GPa Grade Count:46 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |