Mechanical Properties Metric English Comments
Modulus of Elasticity 1.12 - 3.66 GPa
163 - 531 ksi
Average value: 2.69 GPa Grade Count:10
Overview of materials for PVC, Powder
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb..