Polymer Property : Modulus of Elasticity = 0.935 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.00645 GPa
0.935 ksi
ASTM D412 Method A
Seals Eastern 7017 Ethylene-Propylene Rubber
General service EPM.Information provided by Seals Eastern, Inc.
Modulus of Elasticity 0.00645 GPa
0.935 ksi
ASTM D412 Method A
Seals Eastern 7017 Ethylene-Propylene Rubber
General service EPM.Information provided by Seals Eastern, Inc.