Polymer Property : Modulus of Elasticity = 0.750 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.00517 GPa
0.750 ksi
Cured property; ASTM D412
Aptek 2100-A/B Urethane Encapsulant and/or Potting Compound
General purpose encapsulant and potting compound. Outstanding hydrolytic stability. Excellent adhesion to components/circuit boards. Low modulus, low stress. Field proven for military and space appl..