Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.00500 GPa | 0.725 ksi | ASTM D790 |
Premix Thermoplastics PRESEAL® TPE 6080 General Description:PRESEAL® TPE 6080 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It can also be used as conductors or in grounding.. |
|||
Modulus of Elasticity | 0.00500 - 0.338 GPa | 0.725 - 49.0 ksi | Average value: 0.159 GPa Grade Count:54 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |