Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.696 GPa | 101 ksi | Molded Sample 2% Secant Modulus |
Dow DOWLEX™ IP-41 High Density Polyethylene DOWLEX® IP-41 resin is an improved processing high density polyethylene resin designed to offer excellent processability and rigidity required for food containers, overcaps, and other general purpo.. |