Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.00448 GPa | 0.650 ksi | |
Humiseal 1C63 Silicone Conformal Coating Humiseal 1C63 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |