Mechanical Properties Metric English Comments
Modulus of Elasticity 0.614 GPa
89.1 ksi
Molded Sample 2% Secant Modulus
Dow DOWLEX™ IP-40 High Density Polyethylene
DOWLEX® IP-40 resin is an improved processing high density resin designed to offer excellent processability and impact resistance required for food container applications. This resin is designed by..