Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.00314 GPa | 0.455 ksi | ASTM D638 |
Colorite Polymers Elastichem 5511TX-02 Vinyl Compound Description: All components in Elastichem are sanctioned by the U.S. Food & Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulations. For medical use, co.. |